| Specification | Type | Mcp-73 | MP-80 | MCP-75 | MP-81 |
| Chemical composition 5 | Mgo>= | 73 | 80 | 75 | 81 |
| Refractoriness°C | SiO2<= | 4 | 4 | 5 | 3.5 |
| CaO10min 1750min 110°C*24hmin 2.31500°C*3hmax 1.0 | 4max | 10min | 4max | ||
| 1790min | 1750min | 1790min | |||
| Bulk Density g/ m³ | 2.4 | 2.3 | 2.4 | ||
| Linear change | 1.5 | 1.0 | 1.5 | ||
| Critical Grain mm | 3 | 3 | 3 | 3 | |
| Crushing Strength MPa | 1500°C*3h | - | 8min | - | 8min |
| Modulus of Rupture MPs | 1500°C*3h | - | 3min | - | 3min |
| Usage | BOF | BOF | EAF | EAF | |
Calcined Magnesite can be used for Refractory materials, Chemical Industry, Chemical Fertilizer, Construction Materials, Rubber